1.
Mikrobiologiia ; 84(2): 216-24, 2015.
Artigo em Russo | MEDLINE | ID: mdl-26263628

RESUMO

A method for leaching rare earth elements from coal ash in the presence of elemental sulfur using communities of acidophilic chemolithotrophic microorganisms was proposed. The optimal parameters determined for rare element leaching in reactors were as follows: temperature, 45 degrees C; initial pH, 2.0; pulp density, 10%; and the coal ash to elemental sulfur ratio, 10 : 1. After ten days of leaching, 52.0, 52.6, and 59.5% of scandium, yttrium, and lanthanum, respectively, were recovered.


Assuntos
Crescimento Quimioautotrófico/fisiologia , Cinza de Carvão/química , Lantânio/isolamento & purificação , Consórcios Microbianos/fisiologia , Escândio/isolamento & purificação , Ítrio/isolamento & purificação , Acidithiobacillus/metabolismo , Reatores Biológicos , Clostridium/metabolismo , Cinza de Carvão/metabolismo , Concentração de Íons de Hidrogênio , Lantânio/metabolismo , Escândio/metabolismo , Enxofre/metabolismo , Temperatura , Ítrio/metabolismo
SELEÇÃO DE REFERÊNCIAS
DETALHE DA PESQUISA
...